I did 150 then 220 grit sanding and one very heavy coat of Starbright Gold. It looks good, drying a little more in some places than others, but it looks fair to this point. Some say "wetsand" with 400 grit before another coat. Some say clean with mineral spirits and 00 Steel Woo before next coat. I am thinking about putting another coat of Starbright with the Steel Wool as an applicator? Any thoughts on why this is a good or bad idea?